Differential scanning calorimeter (DSC)

Product introduction:

DSC is designed to determine the inner heat transition relating to temperature and heat flow, it is widely used in the field of polymer development, performance testing & quality control. 

More details

Bookmark and Share

DSC research and development includes the following field: glass transition temperature, melting point, cold crystallization, crystallization, phase transition, oxidation induction time (OIT). 

 

Main features:

1. New designed oven structure ensures high resolution and good stability of base line;

2. Air flow meter may control the air flow rate accurately; the test data can be recorded into the database directly;

3. The instrument is bilateral control, may be controlled by both main frame and software. User-friendly interface, easy operation.


Technical parameters:

1. DSC range: 0 ~ ±500mW

2. Temperature range: -100°C~800°C Liquid nitrogen refrigeration

3. Heating rate: 1 ~ 80 °C / min

4. Temperature resolution: 0.1 °C

5. Temperature fluctuations: ±0.1°C

6. Temperature repeatability: ±0.1°C

7. DSC noise: 0.01μW

8. DSC resolution: 0.01μW

9. DSC accuracy: 0.1 u W

10. DSC sensitivity: 0.1 u W

11. Control Mode: Rising temperature, constant temperature, cooling temperature (full automatic programmed control)

12. Curve scanning: Rising scan, *cooling scan

13. Atmosphere control: Embedded digital flow meter & Software control

14. Display:24 bit color  7 inches  LCD touch screen display

15. Data interface: standard USB connector

16. Parameter standard: equipped with standard material, with a key calilbration function, the user may correct temperature and heat enthalpy

17. The warranty: Five years